So I have my envoy coming in about 2 weeks including ACE.  I've come to terms with the low salt level in the water.  What I am still struggling to understand is how it is 'ok' for the water hardness to be 0-50 when using ACE but it is not ok when not using ACE.  What about ACE reduces the leaching of metals by the soft water ? 

Hot Tub Forum

ACE system and low hardness requirement
« on: February 22, 2015, 09:20:40 am »

TwinCitiesHotSpring

  • Full Member
  • ***
  • Posts: 972
Re: ACE system and low hardness requirement
« Reply #1 on: February 22, 2015, 01:30:06 pm »
I run all our ACE equipped spas around 50ppm...all other non ACE spas I try to keep around 100-150...not much difference at all, it keeps any potential calcium deposits away and the "feel" on the skin is much better imo

chem geek

  • Full Member
  • ***
  • Posts: 569
Re: ACE system and low hardness requirement
« Reply #2 on: February 22, 2015, 01:47:48 pm »
There is no "leaching of metals by the soft water".  You only need to provide sufficient calcium hardness (for calcium ions) and total alkalinity and appropriate pH (for carbonate ions) to saturate the water with calcium carbonate when you have plaster/grout surfaces that contain calcium carbonate.  For a spa that is acrylic, there is no need for saturation of the water with calcium carbonate.  The same is true for most vinyl pools.

The idea that saturating the water with calcium carbonate will prevent metal corrosion is very dicey and controversial.  See this discussion among corrosion experts.  Basically, it is very difficult to coat a fine layer of calcium carbonate to protect metal especially when flow rates and temperatures are changing.  Metal corrosion is much more dependent on pH, dissolved oxygen, and the level of other oxidizers.  Some metals such as stainless steel are also affected by the chloride level that interferes with reformation of their oxide passivity layer.

Many municipal water supplies have low calcium hardness (CH).  My water supply has 55 ppm CH and the other water parameters combined have a calcite saturation index of -0.6 yet the copper pipes in all of the serviced homes are not corroding.  There are 300-500 ppb phosphates added to the water as a corrosion inhibitor and is far more effective then trying to saturate the water with calcium carbonate.

So the reason the advice for CH levels is inconsistent is that the advice to have a higher CH in the non-ACE spas is wrong (in terms of metal corrosion).  There really isn't any inconsistency -- there's just wrong advice.  Now, that said, one can reduce foaming in the spa with a higher CH of around 120-150 ppm but that would be incompatible with the ACE system since it needs a very low CH to prevent calcium carbonate buildup on its very sensitive plate material.
« Last Edit: February 22, 2015, 01:58:04 pm by chem geek »

Hot Tub Forum

Re: ACE system and low hardness requirement
« Reply #2 on: February 22, 2015, 01:47:48 pm »

 

Home    Buying Guide    Featured Products    Forums    Reviews    About    Contact   
Copyright ©1998-2024, Whats The Best, Inc. All rights reserved. Site by Take 42